SPE Ntxiv. |
S Ntau dua lossis sib npaug |
FE Ntau dua lossis sib npaug |
SI Tsawg dua los yog sib npaug |
AS Tsawg dua los yog sib npaug |
CU Tsawg dua los yog sib npaug |
ZN Tsawg dua los yog sib npaug |
PB Tsawg dua los yog sib npaug |
H2O Tsawg dua los yog sib npaug |
SIZE Ntau dua lossis sib npaug |
|
S35 |
35% |
30% |
10.0% |
0.01% |
0.01% |
0.5% |
0.15% |
3.0% |
90% |
|
S30 |
30% |
-- |
-- |
0.01% |
0.01% |
0.5% |
0.15% |
3.0% |
90% |
|
SIZE |
(3-35) hli lossis lwm qhov loj |
||||||||
|
PKG |
1000kg / hnab los yog ntau |
||||||||
Core Functions ntawm Pyrite ore lumps nyob rau hauv Roasting rau Precious Hlau rov qab
Muab Qhov Chaw Kub Kub (Autogenous Roasting Roj)
Lumpy pyrite oxidizes thiab tso cua sov ntawm qhov kub siab (600-800 degree):
4FeS₂ + 11O₂ → 2Fe₂O₃ + 8SO₂
Self-combustion tswj qhov kub thiab txias, txo cov roj noj thiab ua kom autogenous roasting.
Oxidative Decomposition ntawm Minerals Liberate Precious Hlau
Cov hlau zoo nkauj (Au, Ag, Pt) feem ntau yog ntim hauv pyrite, arsenopyrite, thiab sulfide ores.
Roasting decomposes thiab oxidizes sulfides, rhuav tshem lawv cov qauv thiab liberating precious hlau los ntawm inclusions rau tom ntej cyanidation / leaching extraction.
Slag Formation thiab Sulfur Fixation rau Form Stable Slag
Roasting tsim Fe₂O₃ (hematite), uas tsim cov hlau-silicate slag nrog gangue minerals (SiO₂, CaO).
Cov slag encapsulates impurities, thaum cov hlau tseem ceeb tseem nyob hauv cov calcine, ua tiav "slag-kub sib cais".
Desulfurization thiab Purification los txhim kho Precious Hlau Qib
Sulfur raug tso tawm raws li SO₂ roj (rov ua dua rau cov kua qaub), thaum impurities xws li arsenic, carbon, thiab organic teeb meem raug oxidized thiab tshem tawm.
Cov qib hlau muaj txiaj ntsig hauv calcine tau nce los ntawm ob peb mus rau kaum ob zaug, txo cov nqi rho tawm tom qab.
Yunfu Pyrite Mine boasts loj ore reserves thiab tso zis, qib siab, tsis muaj impurities, ruaj khov zoo thiab lav lub sij hawm xa tuaj.